Ok guys, I’m breaking down and posting here to see if anyone has any ideas. I’m greatful for any advice.

I have an upgraded flsun SR. I recently lost my computer (psu issue, waiting for replacement) and I took this opportunity to switch from Cura to Orcaslicer.

Over-all I’m very happy, and getting some good speeds, but I just cannot remove stringing no matter what I try:

  • Retraction from 0-7mm. After about 3mm, no further effect
  • Retraction speed from 30mm/s-50mm/s. No noticable effect
  • Travel speed and acceleration both high (up to 350mm/s and 6000 accel. No effect
  • Temp from 205-215 with no effect
  • Dried filament and different colours, no effect
  • Wipe on retract on and off, up to 2mm wipe distance and 100% retraction. No effect
  • Messed with scarf seams on and off, no effect
  • No effect from layer heights

My setup:

  • Printer - FLSun SR running klipper with a speede pad
  • Filament - Esun PLA+
  • Upgrades - Deported fans, OMG v2 extruder, volcano hotend and high flow cht nozzle
  • Rangelus@lemmy.nzOP
    link
    fedilink
    English
    arrow-up
    0
    ·
    7 months ago

    Thanks for the reply mate!

    I didn’t think to mess with z-hop - I’ll give that a go, and I’ll do some testing to make sure the Bowden is seated correctly and the wipe on retract is actually happening - thanks!